How can we extend the usage of RTO blocks to avoid to be damaged? You can do like followings: 1.Try to put the blocks in order when you install the block; 2. Keep expansion gap every 1 centimeter per 1meter evenly distributed when place the blocks; 3. The speed of temperature rise and fall should not be too fast, otherwise it will easily cause cracking in the regenerator product. Within 300°C, the heating rate is ≦ 30°C/h, which mainly excludes adsorbed water; when the temperature is 300-600°C, the rate of temperature rise and fall is 60°C/h, and when the temperature is higher than 600°C, the rate of temperature rise is ≦ 120°C/h; when the temperature is lowered, the temperature is lowered. Speed ≦ 60°C/h; 4.In the working conditions, if there are too many nano-dusts (silicon, organic titanium, etc.), the pores of the regenerator product will be blocked, causing uneven temperature and pressure, and finally leading to product crackin; ...